Sika® Injection-306

Elastic polyacrylic injection resin used for permanent watertight sealing

Sika® Injection-306 is a very low viscous, elastic polyacrylic injection resin with a versatile and adjustable reaction time.

Usage

Packaging

Component A (Resin)

2 × 8.0 kg

Accelerator

1 × 1.0 kg

Hardener powder

4 × 40 g

Measuring cup

1 piece

Advantages

Colour

Component A (Resin)

blue – transparent

Accelerator

yellow – transparent

Hardener powder

white

Additional Accelerator 4 x 1 kg - used for faster reaction times

Product Details

APPROVALS / STANDARDS
  • Wissbau No. 2002-094-(1A) – Function test with SikaFuko® VT 1
  • Wissbau No. 2002-094-(2A) – Function test with SikaFuko® Eco 1
  • FH Aachen – expertise, mechanical long time stability – 01/11/2016
  • MPA TU Braunschweig No. 1200/550/15b – Compatibility Test with Sikaplan WP/WT Membranes 03/02/201
     

Chemical Base

3-part polyacylic resin

 

Shelf Life

12 months shelf life from date of production if stored properly in undamaged, unopened, original sealed packaging.

 

Storage Conditions

Dry storage at temperatures between +10 °C and +30 °C. Protect from direct sunlight and humidity.

 

Viscosity



~3-11 mPa∙s (mixture, at 20 °C)

(acc. ISO 3219)

 
 
 

Application

Mixing Ratio


Accelerator SolutionAccelerator : Watervariable, see Metering Chart below

APremix

Accelerator Solution : Component A (Resin)

2 L per 8 kg of Component A (Resin)

BHardener Solution

Hardener powder : Water

80 g (2 × 40 g) per 10 L of water

Sika® Injection-306

APremix : BHardener Solution

1 : 1 by volume

 

Note for processing in one component pumps:

 

Workability time (pot life) = Reaction time (see metering chart) – 10 minutes

 

Accelerator Metering Chart

ml Accelerator1

Ambient Temperature

 

 

Reaction time

5 °C

(41 °F)

10 °C

(50 °F)

20 °C

(68 °F)

30 °C

(86 °F)

40 °C

(104 °F)

8 min

 

 

2000 2

980 2

380

10 min

 

 

1150 2

480

240

12 min

 

1880 2

820 2

320

180

15 min

1800 2

1240 2

480

220

100

20 min

1060 2

900 2

280

140

60

25 min

820 2

480

200

80

 

30 min

620 2

350

160

  

35 min

440

280

120

  

40 min

360

250

80

  

45 min

320

220

78

  

50 min

250

200

74

 

  1. Quantity of Accelerator per 8 kg component A to, yield of 20 liters kg mixed resin (the Total Accelerator solution must be 2000 ml 2 liters – see example below).
  2. Fast reaction – additional accelerator necessary.

 

Example:
Ambient temperature: 10 °C (50 °F)
Required reaction time: 25 min

Accelerator in ml = 480 ml
Water in ml = 1520 ml
Total volume = 2000 ml

 

Note:
The given data are laboratory parameters and may deviate depending on the object and conditions on site.

 

Ambient Air Temperature


+5 °C min. / +40 °C max

 

Substrate Temperature


+5 °C min. / +40 °C max.

 

Curing Time


8 to 50 minutes

MIXING

  1. Dissolve the content of 2 bags of the hardener powder in 10 litres of water in a separate, clean container. Stir the hardener solution thoroughly until the hardener powder is completely dissolved.
  2. Determine the required quantity of accelerator from the Accelerator Metering Chart (Mixing Ratio), considering the ambient processing temperature and the required reaction time. Dilute the selected quantity of accelerator with water to a total quantity of 2 litres in a separate, clean container.
  3. Pour the 2 litres of accelerator solution into a 8 kg canister of component A (Resin) and mix thoroughly by shaking the canister.

 

The injection resin is activated depending on the type of injection pump used:

 

  • When using a one-component pump: Pour partial amount of the premixed components in a ratio of 1:1 by volume into a clean mixing container and mix mechanically.
  • When using a two-component pump: Fill partial amounts of the premixed components into the storage container of the pump. Set the pump to work at amixing ratio of 1:1 by volume.

 

CLEANING OF TOOLS


Clean all tools and application equipment according to the Product Data Sheet for the Sika® Injection Cleaning System.

 

Document